Zirconia Toughened Alumina Beads

Zirconia Toughened Alumina Beads

Composition(wt%):94.6% ZrO₂+5.4% Y₂O₃

Specific density(g/cm³)≥6.02

Wear rate(ppm)<20(g/kg·h)

Features

  Low abrasion:Pevent material from contamination,guarantee its purity and quality.

  High grinding efficiency:Zirconia grinding medium has the highest efficiency and lowest abrasion in the whole grinding media market.

  Long using life:Lower total cost compared with other grinding media.

  Good stability:Corrosion resistance,can be used in acidic and alkaline material.

Specification

Chemical composition

ZrO₂ 65% SiO₂ 35%

Size (mm)

Real density

4.0g/cm³

0.6-0.8  0.8-1.0

1.0-1.2  1.2-1.4

1.4-1.6  1.6-1.8

1.8-2.0  2.0-2.5

2.5-3.0...............

 

Bulk density

2.69g/cm³

Moh’s hardness

8

Wear rate per ton

0.03kg/h

color

White

package

25kg/barrel

 

Application
  •   For the milling and dispersing of all types of material,widely used in ball mill,vibration mill,planetary mill,stirred mill and high-speed sand mill.

      Non-polluting areas:Food,medicine,cosmetics and other industries.

      Emerging industries:Grinding and dispersing of high purity ultrafine nano material.

      Other industries:Structure ceramics,electronic ceramics,battery material,biomaterials,magnetic material,refractory materials,metallurgy,mining,inks,paints,pigment,etc.